       A240TYPE 304PLATE 입고검사중에 궁금한점이 있어서 질의드립니다.

       ASTM A480/480M Para 10.2항, 13.1.2항에 아래와 같은 내용이 있습니다

10.2  Sheet, Strip, and Plate—For sheet, and strip with No.1 finish and plate with hot-roll anneal

        or hot-roll anneal and pickle finish it is permitted to grind to remove surface imperfections,

        provided such grinding does not reduce the thickness or width at any point beyond the

        permissible variations in dimensions. An iron free abrasive wheel shall be used for such

        grinding and shall be operated at a speed ample to ensure that defective areas are cleanly

        cut out.

13.1.2 Hot-Rolled or Cold-Rolled, and Annealed or Heat Treated, and Blast Cleaned or Pickled

         Condition and finish commonly preferred for corrosion-resisting and most heatresisting

         applications, essentially a No. 1 Finish.

         이 문구의 내용이..
 
         S/S PLATE 생산시 두께나 치수공차 허용범위 내에서 이물질이나 결함을 제거하기 위하여 표면에 Grinder를  

         사용하여도 된다는 내용인지 궁금하네요.

         코드요건이 허용이 된다고 해도 표면은 보기싫은 정도라고 판단이 되네요...  



1321957714&&BBS_FILEmetal.JPG

1321957871&&ADD_FILE1metal.JPG

관리자 2011-11-22 19:43

책에 적힌 것 이상을 적용하려면 항상 무리가 따르지요. Stainless Steel은 가능한 Grind를 대지 않는 게 좋습니다. 한번 Grind를 대게 되면, 전체적으로 Blast Cleaning을 하지 않는 한 계속 그 자욱이 남게 됩니다. 보기싫지요. 이 자욱은 Acid Cleaning을 해도 계속 남아 있어서 보기 싫게 됩니다. Code는 Code문구 그대로 해석해서 적용해야 합니다. 제 생각에는 두께와 관련해서는 위 Code 조항 적용에 문제가 없으나, 현재 요구되는 Surface Finish 조건을 기준으로 위와 같은 상황에 대처하는 게 좋을 듯 합니다. MR이나 기타 관련 Spec.을 보시면 Surface Finish 조건이 있을 겁니다.